ESAB

COREWELD W

COREWELD W

Coreweld W is a metal cored wire designed for single or multipass welding on weathering grade steels. Coreweld W was designed specifically to meet the demand for weld deposits that color match the low alloy, high strength weathering grade steels, such as A588 and A242.

Where To Buy


Industries

  • Ship/Barge Building
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Civil Construction
  • Bridge Construction

Welding Process

  • Welding-MCAW - Metal Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 104 ksi 93 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 23 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCuSCSiNiCr
75% Ar - 25% CO2
PMnCuSCSiNiCr
0.01 %1.2 %0.6 %0.019 %0.06 %0.7 %0.7 %0.6 %

Approvals: DB
Classifications: ASME SFA 5.36; AWS A5.36; E90T15-M21A2-W2; ASME SFA 5.28; AWS A5.28; E80C-W4 H4