Previous Next

ESAB

COREWELD 88HS Ni1

COREWELD 88HS Ni1
  • COREWELD 88HS Ni1
  • COREWELD 88HS Ni1

Coreweld 88HS-Ni1 is recommended primarily for robotic or mechanized high speed welding of sheet steel. Welding speeds up to 90 ipm are possible when welding vertical down. The low slag level of Coreweld 88HS-Ni1 minimizes post weld clean up. For this reason, Coreweld 88HS-Ni1 gives special advantage in applications where post weld coating or painting is specified. Coreweld 88HS-Ni1 is a 1% nickel low alloy metal cored wire designed specifically for high speed welding where a clean weld surface is required. Coreweld 88HS-Ni1 deposits have very few silicon islands and almost no slag at the weld toes.

Add to shopping list


Industries

  • Industrial and General Fabrication
  • Power Poles
  • Railcars

Welding Process

  • Welding-MCAW - Metal Core Arc Welding

Specifications


Typical Tensile Properties

90% Ar - 10% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 26 % 58 % 86.7 ksi 74.3 ksi
75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 27 % 60 % 83.6 ksi 69.6 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 28 ft-lb -50 °F
90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 29 ft-lb -50 °F

Typical Weld Metal Analysis %

90% Ar - 10% CO2
PMnSCSiNi
0.011 %1.31 %0.017 %0.051 %0.61 %0.96 %
75% Ar - 25% CO2
PMnSCSiNi
0.010 %1.23 %0.016 %0.053 %0.55 %0.96 %

Approvals: CWB, CSA W48 E551C-Ni1-H4
Classifications: ASME SFA 5.36, ASME SFA 5.28, AWS A5.36, E80T15-M20A5-Mi1-H4, AWS A5.36, E80T15-M21A5-Ni1 H4, AWS A5.28, E80C Ni1M H4

Approvals are based on factory location. Please contact ESAB for more information.