Coreweld 70 is a tubular wire containing ingredients primarily comprised of metal powder along with additional arc stabilizers and alloying elements. The net result is a high efficiency (90 to 98%) wire. Arc characteristics, weld metal transfer, spatter levels are improved, while silica islands are minimized with the use of Argon mixtures up to 92% Argon. Due to the high level of iron powder and low slag components, the only slag formed by this wire are small islands of silica. Coreweld 70 was designed for multipass welding in robotic applications where slag removal between passes is difficult. This metal cored product is intended for use on carbon steels having tensile strengths up to 70 ksi (485 MPa). Coreweld 70 wires from .045" up to 1/16" are capable of being welded out-of-position.

Add to shopping list


Industries

  • Automotive
  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Pipeline
  • Power Generation
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-MCAW - Metal Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 28 % 67 % 80 ksi 68 ksi
92% Ar - 8% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 26 % 65 % 85 ksi 79 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 50 ft-lb 0 °F
As Welded 40 ft-lb -20 °F
92% Ar - 8% CO2
Condition Impact Value Testing Temperature
As Welded 60 ft-lb 0 °F
As Welded 50 ft-lb -20 °F

Typical Weld Metal Analysis %

92% Ar - 8% CO2
PMnCSSi
0.009 %1.5 %0.06 %0.019 %0.6 %
75% Ar - 25% CO2
PMnCSSi
0.010 %1.4 %0.06 %0.019 %0.6 %

Approvals: CWB, CSA W48 E491C-6M-H4, DB
Classifications: ASME SFA 5.36, ASME SFA 5.18, AWS A5.36, E70T15-M20A2-CS1-H4, AWS A5.36, E70T15-M21A2-CS1-H4, AWS A5.18, E70C-6M-H4