Previous Next

ESAB

COREWELD C6

COREWELD C6
  • COREWELD C6
  • COREWELD C6

Coreweld C6 was developed and "fine-tuned" especially for hand-held, automatic and robotic welding in the automotive industry, as well as rail car manufacturing, structural welding and other similar applications. Never before has there been such a perfect pairing of filler metal and industry requirements for quality, productivity and profitability.

Add to shopping list


Industries

  • Automotive
  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-MCAW - Metal Core Arc Welding

Specifications


Typical Tensile Properties

90% Ar - 10% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 25 % 63 % 86 ksi 79 ksi
75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 27 % 64 % 86 ksi 74 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 43 ft-lb -40 °F
As Welded 56 ft-lb -20 °F
90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 56 ft-lb -20 °F

Typical Weld Metal Analysis %

90% Ar - 10% CO2
PMnSCSi
0.015 %1.6 %0.017 %0.04 %0.8 %
75% Ar - 25% CO2
PMnSCSi
0.012 %1.6 %0.016 %0.04 %0.7 %

Approvals: ABS, CWB, CSA W48 E491C-6M-H4
Classifications: ASME SFA 5.36, ASME SFA 5.18, AWS A5.36, E70T15-M20A2-CS1-H4, AWS A5.36, E70T15-M21A4-CS1-H4, AWS A5.18, E70C-6MD H4