This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD II 100

DUAL SHIELD II 100

Dual Shield II 100 is an all-position flux cored electrode that combines a high strength deposit with excellent impact toughness and low diffusible hydrogen levels. The rutile basic slag system produces a smooth spray-like transfer with reduced spatter and low post weld cleanup. Dual Shield II 100 is designed to join high strength steels such as HY-80 and T-1 the as welded or stress relieved condition using a 75% Ar / 25% CO2 shielding gas. It is especially well suited for high tensile steels that are used in sub-zero temperatures. The weld metal analysis is similar to an E10018-M low hydrogen electrode.

Where To Buy


Industries

  • Mobile Equipment
  • Industrial and General Fabrication

Welding Process

  • FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 22 % 60 % 1050 °F 1 hr 110 ksi 99 ksi
As Welded 21 % 60 % - - 109 ksi 101 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 33 ft-lb 1050 °F 1 hr 0 °F
Stress Relieved 30 ft-lb 1050 °F 1 hr -20 °F
As Welded 32 ft-lb - - -40 °F
As Welded 28 ft-lb - - -60 °F
As Welded 48 ft-lb - - 0 °F
As Welded 40 ft-lb - - -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSiNi
75% Ar - 25% CO2
PMnMoCSSiNi
0.012 %1.45 %0.40 %0.05 %0.01 %0.44 %1.70 %

Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E101T1-M21A2-K3C-H4; AWS A5.29; E101T1-K3M-H4