This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD II 100-D1

DUAL SHIELD II 100-D1

Dual Shield II 100-D1 is an all-position flux cored electrode specially formulated to weld quenched and tempered steels that require a postweld heat treatment using 75% Ar / 25% CO2 shielding gas. Dual Shield II 100-D1 was designed to weld oil field components made of 4130, 8630, API X-80 and similar steels.

Where To Buy


Industries

  • Mobile Equipment
  • Industrial and General Fabrication
  • Civil Construction

Welding Process

  • FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 26 % 58 % 1175 °F 8 hr 94 ksi 85 ksi
As Welded 23 % 58 % - - 102 ksi 94 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 20 ft-lb 1175 °F 8 hr -25 °F
As Welded 33 ft-lb - - -40 °F
As Welded 40 ft-lb - - -25 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSiNi
75% Ar - 25% CO2
PMnMoCSSiNi
0.009 %1.60 %0.33 %0.06 %0.01 %0.40 %0.82 %

Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E101T1-M21A4-D1; AWS A5.29; E101T1-GM