DUAL SHIELD II 101-TC

DUAL SHIELD II 101-TC

Dual Shield II 101-TC is an all-position flux cored electrode developed to meet the U.S. Navy qualification tests for hydrogen levels of less than 0.05 ml/g of deposited weld metal. This unique formulation designed for CO2 shielding optimizes performance and reduces post-weld cleanup cost. Dual Shield II 101-TC produces exceptional mechanical properties and low temperature impact toughness. It is intended for use on HY-80, ASTM A710, A514, and A517 or other similar HSLA steels.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 25 % 94 ksi 87 ksi
As Welded 23 % 103 ksi 93 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 77 ft-lb 0 °F
As Welded 43 ft-lb -60 °F

Typical Weld Metal Analysis %

100% CO2
PMnCSSiNi
0.014 %1.32 %0.03 %0.01 %0.35 %1.64 %

Approvals: DNV-GL; QPL-24403/2; MIL-101TC
Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E91T1-C1A6-K2-H4; AWS A5.29; E91T1-K2C-H4