This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD II 101H4M

DUAL SHIELD II 101H4M

Dual Shield II 101H4M is one of a series of low hydrogen flux cored electrodes introduced by ESAB. Each of the new Dual Shield II H4 wires is an all-position flux cored electrode that provides excellent low temperature toughness in both the as welded and/or stress relieved conditions (as applicable) when used with 75% Ar/25% CO2. Each can produce diffusible hydrogen levels of < 4mL/100g deposited over a wide range of welding parameters. Dual Shield II 101H4M is especially designed to weld HY-80 and HSLA-100 steels typically used in shipbuilding. Suitable for single or multi-pass welding applications. This wire was developed to meet the stringent requirements of MIL-E-24403/2 and offshore welding, and it is an ideal choice for HSLA steels.

Where To Buy


Industries

  • Ship/Barge Building
  • Pipeline
  • Mobile Equipment
  • Industrial and General Fabrication

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 23 % 67 % 102 ksi 93 ksi
As Welded 27 % 68 % 101 ksi 86 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 70 ft-lb 0 °F
As Welded 50 ft-lb -60 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSiNi
75% Ar - 25% CO2
PMnCSSiNi
0.012 %1.37 %0.059 %0.010 %0.36 %2.09 %

Approvals: ABS; QPL-24403/2; MIL-101TM
Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E91T-M21A6-K2H4; AWS A5.29; E91T1-GM-H4