Gas
Equipment -
Arc Gouging (CAC-A) & Exothermic
Cutting -
Welding Automation &
Robotics -
Filler
Metals -
Arc Welding
Equipment - Plasma
-
Cutting
Automation -
Steel Industry
Products -
PPE &
Accessories
- All categories
- Plasma Transferred Arc & Laser Cladding (PTA)
- Covered (Stick) Electrodes (SMAW)
- Gas-Shielded Flux-Cored Wires (FCAW)
- Self-Shielded Flux-Cored Wires (FCAW)
- Metal-Cored Wires (MCAW)
- TIG Rods (GTAW)
- MIG/MAG Wires (GMAW)
- Submerged Arc Wires & Fluxes (SAW)
- Repair and Maintenance
- Ceramic BackUp Tape

ATOM ARC 8018

Atom Arc 8018 electrodes deposit 1% Ni weld metal. They are used primarily to weld high-tensile steels in the 70-80 ksi (483-552 MPa) tensile strength range, especially where notch toughness at temperatures as low as -40°F (-40°C) is required.
Industries
- Bridge Construction
- Industrial and General Fabrication
- Mobile Equipment
- Petrochemical
- Pipeline
- Power Generation
- Ship/Barge Building
Welding Process
- Welding-SMAW/MMA (Stick)