ATOM ARC 8018

ATOM ARC 8018

Atom Arc 8018 electrodes deposit 1% Ni weld metal. They are used primarily to weld high-tensile steels in the 70-80 ksi (483-552 MPa) tensile strength range, especially where notch toughness at temperatures as low as -40°F (-40°C) is required.


Industries

  • Bridge Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Petrochemical
  • Pipeline
  • Power Generation
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Classifications: ASME SFA 5.5, AWS A5.5, E8018-C3 H4R
Approvals: ABS, 3Y/AWS A5.5: E8018-C3, CWB CSA W48, E5518-C3, LR, 4Y40M(H10), QPL-22200/1, MIL-8018-C3

Approvals are based on factory location. Please contact ESAB for more information.


Typical Weld Metal Analysis %

NiPSSiCMnMo
0.97 %0.011 %0.009 %0.33 %0.046 %1.11 %0.13 %

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
As Welded 124 ft-lb -20 °F - -
As Welded 114 ft-lb -40 °F - -
Stress Relieved 129 ft-lb -20 °F 1150 °F 8 hr
Stress Relieved 115 ft-lb -40 °F 1150 °F 8 hr

Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 30 % 1150 °F 8 hr 81 ksi 70 ksi
As Welded 30 % - - 85 ksi 74 ksi