This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD II 81-K2

DUAL SHIELD II 81-K2

The wire produces a smooth stable arc and low spatter levels using a 100% CO2 shielding gas. Dual Shield II 81-K2 was developed for higher tensile steels such as ASTM A302, A533 Class I and A537. Applications include ship fabrication, offshore oil rigs, and heavy equipment construction. This wire is an excellent choice for welding ASTM steels A302, A533 Class I and A537. Dual Shield II 81-K2 produces a smooth stable arc and low spatter levels using 100% CO2 shielding gas. Applications include ship building, offshore oilrigs, and heavy equipment construction.

Where To Buy


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 27 % 73 % 82 ksi 74 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 100 ft-lb 0 °F
As Welded 89 ft-lb -20 °F
As Welded 60 ft-lb -60 °F

Typical Weld Metal Analysis %

PMnSCSiNi
0.013 %1.18 %0.009 %.025 %0.49 %1.44 %

Approvals: ABS, 5Y400SA, H5 (C1), KR, BV, SA5Y50/SA5Y40 H5, KR, CCS, 5Y42SH5, KR, CE, EN 13479, KR, ClassNK, KSWL3G(C)H5, KSW54Y40G(C)H5 (C1), KR, DNV, V Y40MS H5 (C1), KR, GL, 6Y40H5S (C1), KR, KR, L3SG(C) H5 & 5Y40SG(C) H5, KR, LR, 5Y40S H5 (C1), KR, RINA, 5YS H10 (C1), KR
Classifications: ASME SFA 5.36, ASME SFA 5.29, AWS A5.36, E81T1-C1A6-K2-H8, AWS A5.29, E81T1-K2C-H8

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: C Mn Ni
Welding Current: DC+