DUAL SHIELD B6

Dual Shield B6 is an all-position flux cored electrode designed for using with 75% Ar / 25% CO2 or 100% CO2 shielding gas. Dual Shield B6 is intended for use on pipe and plate steels having a nominal 5% chromium - 0.5% molybdenum composition. These steels are typically used in process piping in the oil, gas, petrochemical, and marine industries.

Where To Buy


Industries

  • Pipeline
  • Petrochemical
  • Power Generation

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 20 % 1375 °F 2 hr 98 ksi 84 ksi
100% CO2
Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 20 % 1375 °F 2 hr 93 ksi 78 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoSCSiCr
75% Ar - 25% CO2
PMnMoSCSiCr
0.006 %0.50 %0.50 %0.007 %0.05 %0.70 %5.40 %

Classifications: AWS A5.36; E81T1-C1PZ-B6; ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E81T1-M21PZ-B6; AWS A5.29; E81T1-B6C/E81T1-B6M