DUAL SHIELD 8000-B2L

Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1275 °F 1 hr 87 ksi 76 ksi

Typical Weld Metal Analysis %

PMnMoSCSiCr
0.010 %0.90 %0.50 %0.010 %0.02 %0.40 %1.40 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%) Voltage Wire Feed Speed
.045 in.
1.2 mm
330 A 12.7 lb/h
5.76 kg/h
87 % 34 V 600 in./min
1524 cm/min
.052 in.
1.4 mm
155 A 4.4 lb/h
2 kg/h
87 % 25 V 150 in./min
381 cm/min
.052 in.
1.4 mm
245 A 7.3 lb/h
3.31 kg/h
86 % 28 V 250 in./min
635 cm/min
.052 in.
1.4 mm
310 A 10.2 lb/h
4.63 kg/h
85 % 33 V 350 in./min
889 cm/min
.052 in.
1.4 mm
360 A 13.3 lb/h
6.03 kg/h
85 % 36 V 450 in./min
1143 cm/min
.052 in.
1.4 mm
430 A 17.6 lb/h
7.98 kg/h
87 % 37 V 600 in./min
1524 cm/min
1/16 in.
1.6 mm
190 A 6.1 lb/h
2.77 kg/h
87 % 27 V 150 in./min
38 cm/min
1/16 in.
1.6 mm
300 A 10.2 lb/h
4.63 kg/h
87 % 30 V 250 in./min
35 cm/min
1/16 in.
1.6 mm
365 A 12.3 lb/h
5.58 kg/h
86 % 33 V 300 in./min
762 cm/min
1/16 in.
1.6 mm
410 A 14 lb/h
6.35 kg/h
88 % 33 V 350 in./min
889 cm/min
1/16 in.
1.6 mm
450 A 16 lb/h
7.3 kg/h
87 % 33 V 400 in./min
1016 cm/min
1/16 in.
1.6 mm
500 A 20.1 lb/h
9.11 kg/h
87 % 39 V 500 in./min
1270 cm/min
.045 in.
1.2 mm
150 A 4.2 lb/h
1.91 kg/h
86 % 28 V 200 in./min
508 cm/min
.045 in.
1.2 mm
210 A 6.3 lb/h
86 kg/h
86 % 29 V 300 in./min
762 cm/min
.045 in.
1.2 mm
250 A 8.5 lb/h
3.86 kg/h
87 % 30 V 400 in./min
1016 cm/min
.045 in.
1.2 mm
290 A 10.7 lb/h
4.85 kg/h
87 % 33 V 500 in./min
1270 cm/min

Classifications: ASME SFA 5.36, ASME SFA 5.29, AWS A5.36, E81T1-M21PZ-B2L, AWS A5.29, E81T1-B2LM