ESAB

DUAL SHIELD 8000-B2L

DUAL SHIELD 8000-B2L

Dual Shield 8000-B2L is an all-position flux cored electrode for low carbon grades of 1.25% Cr - 0.5% Mo steels. It is designed for use with 75% - 90% Argon, remainder CO2 shielding gases. The weld metal analysis is similar to an E8018-B2L low Hydrogen electrode.

Where To Buy


Industries

  • Pipeline
  • Petrochemical
  • Chemical Industry

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1275 °F 1 hr 87 ksi 76 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoSCSiCr
75% Ar - 25% CO2
PMnMoSCSiCr
0.010 %0.90 %0.50 %0.010 %0.02 %0.40 %1.40 %

Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E81T1-M21PZ-B2L; AWS A5.29; E81T1-B2LM