DUAL SHIELD 8000-B2

DUAL SHIELD 8000-B2

Dual Shield 8000-B2 is an all-position flux cored electrode which contains 1.25% Cr - 0.5% Mo. The analysis is very similar to Dual Shield 88 CM, except 8000-B2 is for out-of-position welding. The weld metal analysis is similar to an E8018-B2 low Hydrogen electrode. Dual Shield 8000-B2 wire is used for the welding of such steel as 0.5% Cr - 0.5% Mo, 1% Cr-0.5% Mo, and 1.25% Cr - 0.5% Mo. This wire is designed for single or multiple pass welding. Shielding gases of 100% CO2 and 75% Ar - Remainder CO2 may be used.

Where To Buy


Industries

  • Petrochemical
  • Pipeline
  • Power Generation

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 22 % 1275 °F 1 hr 99 ksi 86 ksi
75% Ar - 25% CO2
Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 1275 °F 8 hr 94 ksi 81 ksi

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnMoSCSiCr
0.009 %0.70 %0.50 %0.008 %0.06 %0.60 %1.30 %

Classifications: AWS A5.36; E81T1-M21PZ-B2; ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E81T1-C1PZ-B2; AWS A5.29; E81T1-B2C/E81T1-B2M