This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD 9000-C1

DUAL SHIELD 9000-C1

Dual Shield 9000-C1 is an all-position flux cored electrode which produces a 2.5% Ni deposit. The analysis is very similar to the Dual Shield T-90C1 except that this product has out-of-position capability. Dual Shield 9000-C1 is used for welding of 2-3% Ni steels and castings used in applications requiring good toughness at subzero temperatures. Shielding gas 100% CO2 and 75% Ar - Remainder CO2 may be used.

Where To Buy


Industries

  • Process
  • Ship and Offshore Yards

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 24 % 98 ksi 89 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 25 % 96 ksi 85 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 33 ft-lb -40 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 38 ft-lb 0 °F
As Welded 30 ft-lb -40 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSiNi
75% Ar - 25% CO2
PMnSCSiNi
0.014 %1.50 %0.011 %0.08 %0.70 %2.60 %

Classifications: AWS A5.36; E91T1-M21A4-Ni2; ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E91T1-C1A4-Ni2; AWS A5.29; E91T1-Ni2C/E91T1-Ni2M