Previous Next

ESAB

DUAL SHIELD 810X-NI1

DUAL SHIELD 810X-NI1

Dual Shield 810X-Ni1 provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 810X-Ni1 is designed for use with 100% CO2. It is an excellent choice for welding on COR-TEN® steel in applications where weathering grade wires are not desirable.

Where To Buy


Industries

  • Barges
  • Bridge Construction
  • Civil Construction
  • Heavy Equipment
  • Industrial and General Fabrication
  • Light Equipment
  • Power Generation
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 92 ksi 86 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 60 ft-lb -20 °F
As Welded 45 ft-lb -40 °F

Typical Weld Metal Analysis %

100% CO2
PMnSCSiNi
0.010 %1.30 %0.009 %0.04 %0.60 %1.00 %

Approvals: CWB, CSA W48 E551T1-Ni1C-H8, Seismic Certified "D"
Classifications: ASME SFA 5.36, ASME SFA 5.29, AWS A5.36, E81T1-C1A4-Ni1-H8, AWS A5.29, E81T1-Ni1CD-JH8