DUAL SHIELD 7000-A1

DUAL SHIELD 7000-A1

Dual Shield 7000-A1 is an all-position flux cored electrode recommended for 0.5% Mo steels. It is used in the fabrication and erection of boilers, pressure piping and tubing and other pressure vessel applications. Shielding gas of 100% CO2 and 75% Ar, remainder CO2 may be used. The weld metal analysis is similar to an E7018-A1 low hydrogen electrode.

Where To Buy


Industries

  • Mobile Equipment
  • Power Generation
  • Ship/Barge Building
  • Civil Construction
  • Industrial and General Fabrication

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 26 % 1150 °F 1 hr 93 ksi 82 ksi
As Welded 22 % - - 92 ksi 82 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSi
0.01 %0.90 %0.55 %0.05 %0.01 %0.60 %

Classifications: ASME SFA 5.36; AWS A5.36; E81T1-C1PZ-A1; AWS A5.36; E81T1-C1AZ-A1; ASME SFA 5.29; AWS A5.29; E81T1-A1C/A1M