This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD T-75

DUAL SHIELD T-75

Dual Shield T-75 is a flux cored wire with a basic slag system designed for multiple pass welding and produces excellent properties in both the as welded and stress relieved conditions. The exceptional impact toughness and low sensitivity to cracking makes it an ideal choice for a variety of low and medium carbon steels. The arc characteristics are globular, but can be improved with argon gas mixtures. The weld metal analysis is similar to an E7018 low hydrogen electrode.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Railcars
  • Mobile Equipment
  • Civil Construction

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 29 % 66 % 86 ksi 73 ksi
100% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 28 % 65 % 82 ksi 72 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 55 ft-lb -40 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 70 ft-lb -40 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSi
75% Ar - 25% CO2
PMnSCSi
0.004 %1.70 %0.011 %0.04 %0.70 %

Approvals: ABS; DNV-GL; (3/32"); LR; QPL-24403/1; MIL-70T-5C (3/32")
Classifications: ASME SFA 5.36; ASME SFA 5.20; AWS A5.36; E70T5-M21-CS1-H4; AWS A5.36; E70T5-C1A4-CS1-H4; AWS A5.20; E70T-5C-JH4/T-5M-JH