DUAL SHIELD II 711X

DUAL SHIELD II 711X

Dual Shield II 711X is an all-position flux cored wire that displays exceptional impact properties in combination with CO2 shielding gas. This flux cored wire was developed to join low and medium carbon steels where higher impacts and toughness are required. As with all X Series wires, Dual Shield II 711X offers higher top-end current levels for out-of-position welding, broader operating ranges and higher deposition rates in out-of-position applications. Applications include construction, shipbuilding, rail car, light and heavy equipment, and general fabrication where exceptional impacts are required. Weld metal analysis is similar to Atom Arc 7018 and Atom Arc 7018-1.

Where To Buy


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 86 ksi 78 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 96 ft-lb 0 °F
As Welded 79 ft-lb -20 °F
As Welded 36 ft-lb -40 °F

Typical Weld Metal Analysis %

PMnCSSiNi
0.012 %1.4 %0.04 %0.010 %0.4 %0.4 %

Approvals: ABS, CWB, CSA W48 E491T-12-H8, DNV-GL, LR
Classifications: ASME SFA 5.36, ASME SFA 5.20, AWS A5.36, E71T1-C1A4-CS2-DH8, AWS A5.20, E71T-CJ-DH8/T-9CJ-DH8/T-12CJ-DH8