DUAL SHIELD II 71 ULTRA

DUAL SHIELD II 71 ULTRA

Dual Shield II 71 Ultra is an all-position flux cored wire that displays exceptional impact properties when used with CO2. The improved properties qualify this wire to the Navy's "HY" classification. The "Ultra" series produces smoother arc characteristics and lower welding fumes. Dual Shield II 71 Ultra was developed to join low and medium carbon steel. The Military classification allows Dual Shield II 71 Ultra to be used for attaching steels of less than 80 ksi (552 MPa) yield to HY-80 and HY-100. Commercial applications include construction, shipbuilding, railcar, and heavy equipment industries. Weld metal analysis is similar to an E7018 low hydrogen electrode.

Where To Buy


Industries

  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 28 % 77 % 79 ksi 71 ksi

Typical Charpy V-Notch Properties

100% C02
Condition Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
As Welded 72 ft-lb -40 °F - -
100% CO2
Condition Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
Stress Relieved 62 ft-lb -40 °F 1150 °F 1 hr
As Welded 114 ft-lb 0 °F - -
As Welded 98 ft-lb -20 °F - -

Typical Weld Metal Analysis %

PMnSCSi
0.012 %1.40 %0.010 %0.03 %0.40 %

Approvals: ABS, CWB, CSA W48 E491T-12J-H8, DNV-GL, LR, QPL-24403/1, MIL-71T-1C, QPL-24403/1, MIL-71T-1-HYC
Classifications: ASME SFA 5.36, ASME SFA 5.20, AWS A5.36, E71T1-C1P4-CS2-H8, AWS A5.36, E71T1-C1A4-CS2-H8, AWS A5.20, E71T-1CJ-H8/T-9CJ-H8/12CJ-H8