DUAL SHIELD II 70 Ultra

DUAL SHIELD II 70 Ultra

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties when used with 75% Ar/25% CO2. The improved properties qualify this wire to the Navys "HY" classification. The "Ultra" series produces smoother arc characteristics and lower welding fumes. Dual Shield II 70 Ultra was developed to join low and medium carbon steel. The Military classification allows Dual Shield II 70 Ultra to be used for attaching steels of less than 81 ksi (560 MPa) yield to HY-80 and HY-100. Commercial applications include construction, shipbuilding, railcar, and heavy equipment industries.

Where To Buy


Industries

  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 29 % 75 % 81 ksi 72 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 80 ft-lb -40 °F
As Welded 110 ft-lb -20 °F
As Welded 117 ft-lb 0 °F

Typical Weld Metal Analysis %

PMnSCSi
0.008 %1.1 %0.004 %0.03 %0.45 %

Approvals: LR, MIL, 71T-1M, MIL, 71T-1-HYM, ABS, BV, CWB, CSA W48 491T-12M-H8, CL, DNV-GL, DB
Classifications: ASME SFA 5.36, ASME SFA 5.20, AWS A5.36, E71T1-M21A4-CS2-H8, AWS A5.20, E71T1MH8/T9MH8/T12MH8