ATOM ARC 9015-B9

ATOM ARC 9015-B9

Atom Arc 9015-B9 is designed to weld the modified 9% Cr & 1% Mo steels known by the designations T91, P91 or Grade 91. These steels are designed to provide improved creep strength, fatigue, oxidation, and corrosion resistance at elevated temperatures.

Where To Buy


Industries

  • Petrochemical
  • Pipeline
  • Power Generation

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 20 % 1350 °F 1 hr 114 ksi 95 ksi
Stress Relieved 19 % 1375 °F 1 hr 119 ksi 102 ksi
Stress Relieved 23 % 1400 °F 1 hr 106 ksi 86 ksi

Typical Weld Metal Analysis %

MnMoX-FactorCNCrPARCuSNbSiV
0.85 %1.00 %< 15 %0.10 %0.04 %8.60 %0.009 %<0.01 %0.05 %0.009 %0.04 %0.19 %0.21 %