DUAL SHIELD 70 ULTRA PLUS

DUAL SHIELD 70 ULTRA PLUS

Dual Shield 70 Ultra Plus is an all-position wire that is uniquely designed to provide high deposition, outstanding all position performance and a fume emission rate approaching that of solid wires. It is optimized for use with 90% Ar/10% CO2 shielding but works well with mixes ranging from 75% Ar/25% CO2 to 95% Ar/5% CO2. Among the outstanding features of Dual Shield 70 Ultra Plus are a very wide operating window, very high out of position deposition rates (vertical up and overhead at over 12 lb/hr), and welds that are virtually spatter free. Dual Shield 70 Ultra Plus may be used in a variety of applications including railcar, automotive, heavy equipment, and general structural steel fabrication. It is especially recommended in applications where reduction of welding fume is a priority.

Where To Buy


Industries

  • Automotive
  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Process
  • Railcars
  • Ship/Barge Building
  • Steel Industry

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 86 ksi 76 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 53 ft-lb 0 °F
As Welded 40 ft-lb -20 °F
90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 68 ft-lb 0 °F
As Welded 43 ft-lb -20 °F

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnCSSi
0.016 %1.2 %0.04 %0.012 %0.6 %

Approvals: CWB CSA W48, E491T-1M-H16, ABS
Classifications: ISO, 173632-B T493T1-1MA- U, ASME SFA 5.36, ASME SFA 5.20, AWS A5.36, E71T1-M20A2-CS1, AWS A5.36, E71T1-M21A4-CS1, AWS A5.20, E71T-1M/T-9M