DUAL SHIELD 7100 LC

DUAL SHIELD 7100 LC

Dual Shield 7100 LC provides outstanding operator appeal with its easily controlled arc, improved operation at lower current levels, minimal spatter and easily removed slag. Dual Shield 7100 LC can be used with CO2 or 75% Ar/25% CO2 shielding, however pure CO2 is recommended in applications where restraint is high.

Where To Buy


Industries

  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Process
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 26 % 64 % 90 ksi 83 ksi
100% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 23 % 52 % 81 ksi 73 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 50 ft-lb 0 °F
As Welded 31 ft-lb -20 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 68 ft-lb 0 °F
As Welded 41 ft-lb -20 °F

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnCSSi
0.010 %1.4 %0.03 %0.010 %0.6 %
100% CO2
PMnCSSi
0.010 %1.2 %0.03 %0.010 %0.5 %

Approvals: ABS; CWB; CSA W48 E491T-9-H8, E491T-9M-H8; DNV-GL; LR; Seismic Certified "D"
Classifications: ASME SFA 5.36; ASME SFA 5.20; AWS A5.36; E71T1-M21A2-CS1-H8; AWS A5.36; E71T1-C1A4-CS1-DH8; AWS A5.20; E71T-1C-DH8/T-1MH8/T-9C-DH8/T-9MH8