DUAL SHIELD 710X-M

DUAL SHIELD 710X-M

Dual Shield 710X-M provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 710X-M is designed to be used with 75/25 Argon CO2 gas mix.

Where To Buy


Industries

  • Barges
  • Civil Construction
  • Industrial and General Fabrication
  • Light Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 83 ksi 74 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 72 ft-lb 0 °F
As Welded 56 ft-lb -20 °F

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnSCSi
0.012 %1.3 %0.008 %0.04 %0.5 %

Approvals: Seismic Certified "D"; ABS; CWB; CSA W48 E491T-9M-H8; DNV-GL; LR; MIL-E-24403A; 71T-1M
Classifications: ASME SFA 5.36; ASME SFA 5.20; AWS A5.36; E71T1-M21A4-CS1-DH8; AWS A5.20; E71T-1MD-H8/T-9MD-H8