This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD 710X

DUAL SHIELD 710X

Dual Shield 710X is an all-position flux cored wire for general purpose welding. It provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 710X can be used with 100% CO2, recommended in applications where weld joint restraint is high. Applications include rail car, barges, civil construction, light equipment and general fabrication.

Where To Buy


Industries

  • Civil Construction
  • Light Equipment
  • Barges
  • Industrial and General Fabrication
  • Ship/Barge Building
  • Railcars

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 27 % 93 ksi 83 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 87 ksi 75 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 75 ft-lb 0 °F
As Welded 50 ft-lb -20 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 57 ft-lb 0 °F
As Welded 49 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSiNi
75% Ar - 25% CO2
PMnSCSiNi
0.005 %1.5 %0.009 %0.03 %0.6 %0.4 %

Approvals: LR; DNV-GL; CWB; CSA W48 E491T-9-H8; ABS; Seismic Certified “D”
Classifications: ASME SFA 5.36; ASME SFA 5.20; AWS A5.36; E71T1-C1A2-CS1-DH8; AWS A5.20; E71T-1C-DH8/T-9C-DH8