DUAL SHIELD 111-RB

DUAL SHIELD 111-RB

Dual Shield 111-RB is a low slag, high deposition flux cored electrode designed for joining structural components made of low carbon steel and can be used to weld over some primer compositions. The electrode is designed to be used with 100% CO2 gas shielding. Dual Shield 111-RB can achieve deposition efficiency above 88%. This increases the amount of deposit achieved over a given period of time, as compared to a standard Dual Shield E70T-1 electrode.

Where To Buy


Industries

  • Mobile Equipment
  • Industrial and General Fabrication
  • Civil Construction
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 28 % 65 % 87 ksi 75 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 29 ft-lb 0 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSi
100% CO2
PMnCSSi
0.014 %1.5 %0.05 %0.015 %0.04 %

Approvals: ABS; MIL-E-24403/1; 70T-1C
Classifications: AWS A5.36; E80T1-C1A2-CS1; ASME SFA 5.29; ASME SFA 5.36; ASME SFA 5.20; AWS A5.36; E70T1-C1A2-CS1; AWS A5.20; E70T-1C; AWS A5.29; E80T-1GC