This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

DUAL SHIELD 700X

DUAL SHIELD 700X

Dual Shield 700X is a high deposition, deep penetration wire for joining of heavy structural steel components. Designed for flat and horizontal position welding using CO2 shielding gas, this X Series wire provides high deposition rates, high efficiency and excellent performance. The bead contour, smooth ripple and slag chemistry allow easy slag removal even in narrow groves.

Where To Buy


Industries

  • Heavy Equipment
  • Large Components
  • Mobile Equipment
  • Agricultural Equipment

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 87 ksi 79 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 49 ft-lb 0 °F
As Welded 33 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSi
100% CO2
PMnCSSi
0.011 %1.50 %0.035 %0.015 %0.55 %

Approvals: ABS; CWB; CSA W48 E492T-1; DNV-GL; LR
Classifications: ASME SFA 5.36; ASME SFA 5.20; AWS A5.36; E70T1-C1A2-CS1-H8; AWS A5.20; E70T-1CH8/E70T-9CH8