ATOM ARC 8018-B8

ATOM ARC 8018-B8

Atom Arc 8018-B8 is designed to weld 9% Cr - 1% Mo creep resisting steels such as ASTM A213-T9 and A335-P9. These steels are used in pressure vessels and piping for high temperature service.

Where To Buy


Industries

  • Pipeline
  • Power Generation
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 22 % 1375 °F 1 hr 98 ksi 79 ksi

Typical Weld Metal Analysis %

PMnMoX-FactorCSSiCr
0.01 %0.80 %1.00 %< 15 %0.07 %0.01 %0.30 %8.60 %

Classifications: ASME SFA 5.5, AWS A5.5, E8018-B8 H4R