A welding glove with two layers of cowhide capable of withstanding extreme heat – suitable for tubular wire welding. The facing of aluminum-coated PFR rayon reflects 95% of the thermal radiation. Gloves are padded with COMFOflex®, and sewn with fourfold Kevlar®. The thumb is angled for high comfort.

Where To Buy


Features

  • Tested against mechanical stress such as abrasion, cut, tear, and puncture.
  • Tested for thermal performance, such as exposure to an open flame, contact heat, convective heat, radiant heat, and small and large splashes of molten metal.