ATOM ARC 8018-B6

Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1375 °F 1 hr 101 ksi 86 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoX-FactorCSSiCr
0.013 %0.70 %0.60 %< 15 %0.07 %0.009 %0.50 %5.30 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%) Optimal Amps
3/32 in.
2.4 mm
70-100 A 1.7 lb/h
0.8 kg/h
66.3 % 90 A
1/8 in.
3.2 mm
90-160 A 2.6 lb/h
1.2 kg/h
71.6 % 120 A
1/8 in.
3.2 mm
90-160 A 2.7 lb/h
1.2 kg/h
70.9 % 140 A
5/32 in.
4.0 mm
130-220 A 3.1 lb/h
1.1 kg/h
75 % 140 A
5/32 in.
4.0 mm
130-220 A 3.8 lb/h
1.7 kg/h
73.5 % 170 A

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B6 H4R