ATOM ARC 8018-B6

ATOM ARC 8018-B6

Atom Arc 8018-B6 is designed to weld 5% Cr -0.5% Mo creep resisting steels such as ASTM A387 Grade 5, A213-T5 and A335-P5. These steels are normally used in pressure vessels and piping for high temperature service.

Where To Buy


Industries

  • Pipeline
  • Power Generation
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1375 °F 1 hr 101 ksi 86 ksi

Typical Weld Metal Analysis %

PMnMoX-FactorCSSiCr
0.013 %0.70 %0.60 %< 15 %0.07 %0.009 %0.50 %5.30 %

Classifications: ASME SFA 5.5, AWS A5.5, E8018-B6 H4R