The red coated Sureweld 10P is an all-position cellulosic electrode developed for the pipe welding industry in order to improve ductility in the weld deposit while maintaining the standard welding characteristics needed for a pipe welding electrode. Sureweld 10P produces a steady, deep penetrating arc and maintains the proper keyhole in an open root. This electrode will produce X-ray quality joints in flat, horizontal, overhead, vertical-up, and vertical-down procedures. Sureweld 10P is recommended for welding API grades A25, A, B and X42 pipe and general structural, ship, barge and storage tank fabrication. It may also be used for welding root passes in higher grade pipe in some circumstances.

Add to shopping list


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Pipeline

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 79 ksi 67 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 27 ft-lb 0 °F
As Welded 22 ft-lb -20 °F

Typical Weld Metal Analysis %

PMnCSSi
0.01 %0.30 %0.12 %0.02 %0.20 %

Approvals: ABS, AWS A5.1: E6010
Classifications: ASME SFA 5.1, AWS A5.1, E6010

Approvals are based on factory location. Please contact ESAB for more information.


x
×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..