ATOM ARC 8018-B3L

ATOM ARC 8018-B3L

Atom Arc 8018-B3L electrodes contain 2.25% Cr and 1% Mo alloy additions with low carbon content. The electrode is designed for welding 2.25% Cr - 1% Mo steels. The rod operates with a very stable arc and minimal spatter. The low carbon analysis of the weld metal contributes to its crack resistance. The addition of Cr and Mo provide for the excellent creep and stress rupture properties of weldments subjected to elevated temperature service.

Where To Buy


Industries

  • Mobile Equipment
  • Pipeline
  • Power Generation

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 25 % 1275 °F 1 hr 93 ksi 78 ksi

Typical Weld Metal Analysis %

PMnMoCSSiCr
0.017 %0.70 %1.10 %0.04 %0.015 %0.40 %2.30 %

Classifications: ASME SFA 5.5, AWS A5.5, E8018-B3L H4R