This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

PT-31XL / PT-31XLPC Plasmarc Manual Cutting Torches

PT-31XL / PT-31XLPC Plasmarc Manual Cutting Torches

Designed for superior operator comfort, ESABs PT-31XL and PT-31XLPC are the most compact 50 Amp torches on the market.

Where To Buy


Features

  • Excellent cutting capability–manually cuts up to 3/4 in. (19 mm); severs up to 1 in. (25.4 mm)
  • New, durable torch cable prevents snagging on fixtures and materials
  • Equipped with patented safety interlock feature
  • Uses shop air, cylinder air or nitrogen for superior versatility
  • High frequency starting–even starts through paint
  • Uses patented "XT" consumables
  • Consoles|The PT-31XL and PT-31XLPC can be used with the following consoles:
    HandyPlasma 250
    HandyPlasma 380
    HandyPlasma 550
    PowerCut 650

Specifications

Cutting Specifications

Cuts Manual 3/4 in.
Severs Manual 1 in.

Dimensions

Length 5.25 in.

Torch Head

Length 2.25 in.

Output Ratings

Current Capacity @ 100% Duty Cycle

Output Current AC 50 A

Plasma Gas Requirements

Air Supply

Gas Flow 275 cfh (130 l/min)
Gas Pressure 75 psig