Previous Next

ESP-150 Plasmarc Cutting & Gouging System

Specifications


Cutting Specifications

Cuts Manual 2 in.

Dimensions

Height 31.5 in.
Length 40 in.
Width 21.75 in.

Input Ratings

Open Circuit Voltage

VDC 370 VDC
Amps 121/112/70/64/56/45 A
Frequency Hz 50/60 Hz
Phases 3
VAC 220/230/380/415/460/575 VAC

Output Ratings

Duty Cycle 90 %
Output Current AC 150 A
VAC Out 120 VAC
Duty Cycle 100 %
Output Current AC 140 A
VAC Out 120 VAC

Weight

Weight 756 lb