Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 35 % 77 % 1150 °F 16 hr 74 ksi 59 ksi
Stress Relieved 35 % 76 % 1150 °F 8 hr 76 ksi 61 ksi
As Welded 32 % 76 % - - 83 ksi 68 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
As Welded 114 ft-lb -20 °F - -
Stress Relieved 133 ft-lb -20 °F 1150 °F 8 hr
Stress Relieved 185 ft-lb -20 °F 1150 °F 16 hr

Typical Weld Metal Analysis %

PMnMoCSSi
0.014 %1.30 %0.10 %0.06 %0.014 %0.30 %

Classifications: ASME SFA 5.1, AWS A5.1, E7018 H4R