Thermal Dynamics

Cutmaster 58

Cutmaster 58

The Cutmaster 58 is the most powerful 5/8 in. (16 mm) machine on the market today. This unit cuts through mild, stainless, or aluminum up to 1 in. (25 mm) thick. The Cutmaster 58 combines power with the well-known performance and features of the industry-leading 1Torch®.

Where To Buy


Features

  • 6.2 kW rated output, 50% Duty Cycle at 60A, available in 600V and 208-460V with automatic multi-voltage detection
  • Built for portability and durability with the integral multi-handle design
  • SL60QD 1Torch quick disconnect with ATC® (Advanced Torch Connector) allowing selective replacement of either the torch handle assembly or the torch leads, using the patented SureLok® technology also available as an RPT Torch
  • 5/8 in. (16 mm) recommended cut capacity with greater than 1 in. (25 mm) maximum cut and 1/2 in. (13 mm) pierce rating
  • Industry leading 4-year warranty on power supply and 1-year warranty on torch


Industries

  • Civil Construction
  • General Manufacturing
  • Repair and Maintenance

Specifications

Cutting Specifications

Maximum Cut 1 in. (25 mm)
Pierces 1/2 in. (13 mm)
Recommended Cut 5/8 in. (16 mm)

Dimensions

Height 15 in. (381 mm)
Length 24 in. (610 mm)
Width 12 in. (305 mm)

Input Ratings

Frequency Hz 50/60 Hz
Phase 1/3
Volts 208-230/460 V
Frequency Hz 50 Hz
Phase 3
Volts 460 V

Operating Specifications

Operating Temperature 0 - 40 °C (32 - 104 °F)