Purus 42

Purus 42

Purus 42, AWS ER70S-6 wire, is specially formulated to reduce post-welding cleaning. The superior wire composition reduces silica islands and spatter. Purus has excellent arc start ignition, arc stability and significantly less spatter. In robotic and high volume operations, Purus can significantly reduce post welding cleaning time by reducing silica islands and unplanned downtime in multipass welding. It can also increase uptime with longer tip life. With exceptional control of wire composition and the manufacturing process, Purus maintains a stable process between batches.

Where To Buy


Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 24 % 77 ksi 62 ksi
80% Ar - 20% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 25 % 81 ksi 68 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 48 ft-lb -40 °F
As Welded 55 ft-lb -22 °F
As Welded 81 ft-lb 68 °F
80% Ar - 20% CO2
Condition Impact Value Testing Temperature
As Welded 59 ft-lb -40 °F
As Welded 66 ft-lb -22 °F
As Welded 96 ft-lb 68 °F

Typical Weld Metal Analysis %

PMnSCSi
0.020 %1.45 %0.020 %0.085 %0.85 %

Approvals: CWB, CSA W48-14, VdTÜV, 19190, CE EN, 13479
Classifications: EN ISO 14341-A:, G 3Si1, SFA/AWS A5:18:, ER70S-6

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Carbon-manganese steel (Mn/Si-alloyed)