This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

OK Tigrod 5183

OK Tigrod 5183

OK Tigrod 5183 was developed to provide the highest strengths possible in the as welded condition of alloy AA 5083 and other similar high magnesium alloys. The more common OK Tigrod 5356 will typically fail to meet the as-welded tensile requirements of AA 5083. The alloy is typically utilised in marine and structural applications where high strengths, high fracture toughness for impact resistance and exposure to corrosive elements are important. The alloy is not recommended for elevated temperature applications due to its susceptibility to stress corrosion cracking. The alloy is non-heat treatable.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
25 % 42 ksi 20 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
66 ft-lb 68 °F

Typical Weld Metal Analysis %

MnCuZnTiSiMgAlCrFe
0.65 %0.01 %0.01 %0.100 %0.04 %4.9 %94.200 %0.08 %0.13 %

Approvals: ABS, R 5183, CE, EN 13479, CWB, A5.10/A5.10M:2012 ER5183, DB, 61.039.04, JIS, JIS Z 3232, NAKS/HAKC, 3.2MM, VdTÜV, 04667
Classifications: SFA/AWS A5.10, R5183, Wire Electrode, EN ISO 18273, S Al 5183 (AlMg4,5Mn0,7(A)), Wire Electrode, JIS Z 3232, A5183, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMgMn