OK Band 310MoL


Strip for submerged arc and electroslag strip cladding. Together with OK Flux 10.10 is used for electroslag strip cladding giving low carbon "310LMo" material in the second layer. The alloy is fully austenitic and mostly used in urea plants.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnMoCSiFerrite FNNiNCr
4.5 %2.1 %0.02 %0.22 %0 %22.0 %0.13 %25.0 %

Approvals: VdTÜV, 12102
Classifications: EN ISO 14343-A, B 25 22 2 N L

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: 25Cr - 22 Ni - 2 Mo - 5 Mn - N