ESAB

OK Band 309LNb ESW


OK Band 309LNb ESW is a stainless strip for single layer electroslag strip surfacing. Together with OK Flux 10.10 it produces a 347 type of weld deposit.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnCNbSiFerrite FNNiNCr
1.74 %0.01 %0.6 %0.20 %15 %11.0 %0.04 %21.14 %

Approvals: NAKS/HAKC; 30, 60 and 90 mm
Classifications: EN ISO 14343-A; B 22 12 L Nb