OK Band 11.84


A welding strip designed for surfacing using the electroslag strip cladding process.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCSiWNiCr
1.18 %1.7 %0.35 %0.22 %1.8 %0.5 %6.5 %

Alloy Type: 7Cr - Mo - W - with higher C content