OK Autrod NiCrMo-4


OK Autrod NiCrMo-4 is a corrosion and heat resistant, nickel-chromium wire for submerged arc welding of high alloyed steel, heat resistant steel, corrosion resistant steel, 9Ni steels and similar steels with high notch toughness at low temperatures. OK Autrod NiCrMo-4 can be combined with OK Flux 10.90 or OK Flux 10.16.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnMoCSiWNiCrFe
0.45 %16.1 %0.01 %0.05 %3.5 %Bal. %15.5 %5.8 %

Classifications: SFA/AWS A5.14, ERNiCrMo-4, Wire Electrode, EN ISO 18274, S Ni 6276 (NiCr15Mo16Fe6W4), Wire Electrode