OK Autrod NiCrMo-3


Ni-based solid wire for SAW welding. Corrosion and heat resistant. For welding of high alloyed steels, heat resistant steels, corrosion resistant steels, 9% Ni-steels and similar steels with high toughness at low temperatures. OK Autrod NiCrMo-3 shall be combined with OK Flux 10.90 or OK Flux 10.16.

Where To Buy


Specifications


Typical Weld Metal Analysis %

MnMoCSiNiNb+TaCrFe
0.04 %8.6 %0.02 %0.06 %bal %3.5 %22.7 %0.3 %

Classifications: SFA/AWS A5.14, ERNiCrMo-3, Wire Electrode, EN ISO 18274, S Ni 6625 (NiCr22Mo9Nb), Wire Electrode