OK Autrod NiCrMo-13


OK Autrod NiCrMo-13 is a Nb-free, Ni-Cr-Mo wire for welding high-alloyed steels of the 20Cr25Ni4-6Mo type and nickel-based alloys of similar type. The wire can also be used for welding these steels with dissimilar steels. The weld metal has very good corrosion resistance in both oxidizing and reducing media. OK Autrod NiCrMo-13 can be combined with OK Flux 10.90 or OK Flux 10.16.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnMoCSiNiAlCrFe
0.2 %16.0 %0.01 %0.1 %bal %0.3 %23.0 %1.0 %

Classifications: SFA/AWS A5.14, ERNiCrMo-13, Wire Electrode, EN ISO 18274, S Ni 6059 (NiCr23Mo16), Wire Electrode