ESAB

OK Autrod 310MoL


A continous solid corrosion resisting chromium-nickel-molybdenum wire for welding of austenitic manganese steels of 25% Cr, 22% Ni, 2% Mo types. OK Autrod 310MoL has a good resistance to pitting, intergranular corrosion and stress corrosion cracking. The alloy is used in acid rich environments, in the urea industry and in gas treatment plants. OK Autrod 310MoL can be used in combination with OK Flux 10.93.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCSiFN WRC-92NiNCr
4.5 %2.0 %0.01 %0.1 %0 %22.0 %0.14 %25.0 %

Classifications: EN ISO 14343-A; S 25 22 2 N L; Wire Electrode

Alloy Type: Austenitic (25% Cr - 22% Ni - 2% Mo - nitrogen - low carbon)