Specifications


Typical Charpy V-Notch Properties

As welded
Testing Temperature
-20 °C
-50 °C

Typical Charpy V-Notch Properties

As welded
Testing Temperature
-20 °C
-50 °C

Typical Weld Metal Analysis %

MnMoCSiNiNCr
0.78 %2.8 %0.016 %0.63 %8.6 %0.13 %21.7 %

Approvals: CE, EN 13479, VdTÜV, 09775
Classifications: EN 14700, T Fe11, Weld Metal, SFA/AWS A5.9, EC2209, Weld Metal, EN ISO 17633-A, T 22 9 3 N L M M12 2, Weld Metal, EN ISO 17633-A, T 22 9 3 N L M M13 2, Weld Metal