ESAB

ATOM ARC 7018 Acclaim

ATOM ARC 7018 Acclaim

Atom Arc 7018 Acclaim offers the deep, penetrating arc and tough mechanical properties of the original Atom Arc 7018 with greater puddle control resulting in ease of use in out-of-position welding applications and superior arc initiation desired by many newer welders. Both novice and seasoned welders can appreciate its excellent weld performance, wide operating range and easy clean up. Greater puddle control resulting in easier out-of-position welds, superior arc initiation and ease of use with wider operating range and minimal clean-up

Where To Buy


Industries

  • Civil Construction
  • Mobile Equipment
  • Ship/Barge Building
  • Bridge Construction
  • Railcars
  • Automotive
  • Industrial and General Fabrication

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 32 % 86.9 ksi 72.4 ksi
As Welded 36 % 79 ksi 65 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 85 ft-lb -50 °F
As Welded 170 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSi
0.01 %1.20 %0.05 %0.008 %0.45 %

Approvals: LR; 4Ym (H5); ABS; 4Y (H5)/AWS A5.1: E7018 H4R; DNV/GL; 4Y (H5); CWB CSA W48; E4918-1-H4
Classifications: ASME SFA 5.1; AWS A5.1; E7018 H4R

Approvals are based on factory location. Please contact ESAB for more information.